MY字典>英语词典>striation翻译和用法

striation

英 [straɪˈeɪʃn]

美 [straɪˈeɪʃn]

n.  (尤指肌肉上的)条纹

复数:striations 

医学

BNC.44088 / COCA.30678

牛津词典

    noun

    • (尤指肌肉上的)条纹
      a striped pattern on sth, especially on a muscle

      英英释义

      noun

      • a stripe or stripes of contrasting color
        1. chromosomes exhibit characteristic bands
        2. the black and yellow banding of bees and wasps
        Synonym:bandbandingstria
      • any of a number of tiny parallel grooves such as: the scratches left by a glacier on rocks or the streaks or ridges in muscle tissue
          Synonym:stria

        双语例句

        • Shape-reconstruction to discrete point cloud data sampling from the striation figure is one of important research contents of it.
          针对采样于线状图形的离散点云数据的形状重建是其中的重要研究内容之一。
        • The fatigue fracture characteristics were fatigue striation, ductile microvoid, and quasi-cleavage-like fracture characteristic.
          疲劳断裂特征为疲劳条纹、韧窝及类似准解理状形貌特征。
        • The spectrum radiance in bright and dark region of striation discharge is studied experimentally.
          实验研究了条纹放电的明条纹和暗条纹中汞原子的谱线强度。
        • A model of generation of striation based on the diffusion reaction of iron and oxygen was given.
          提出了一种基于铁和氧气扩散反应进行的管材激光切割表面条纹形成模型。
        • The crack celerity expand to form the fatigue striation when puff part adequacy long in the positive stress.
          当断面张开部分足够长时,在正向应力作用下发生快速扩展,微观形成疲劳辉纹。
        • They need to inspect the metal for definitive signs of striation marks ( which would be consistent with chemical explosive, like Semtex, which they quickly discovered on the inside of the fuselage of Pan Am 103) and for the shape of the metal.
          他们要检查金属是否有确切的波纹痕迹(波纹痕迹意味着化学品爆炸,如塞姆汀炸药,当年调查人员在泛美103航班的机身内部很快就发现了这种炸药)以及金属机身的形状。
        • Objective To introduce a method for examination of striation marks left by claw-hammer.
          目的介绍羊角锤起钉槽撬压形成擦划痕迹的检验方法。
        • The striation spacing in heat affect zone and welded seam samples was wider than that in matrix sample, this shows that fatigue crack propagation resistance of heat affect zone and welded seam was smaller than that of matrix.
          焊缝区和热影响区试样的辉纹间距较基体区的大,说明裂纹扩展速率快,焊缝和热影响区的抗裂纹扩展性较基体差。
        • And formation of typical fatigue striation on fatigue crack steady propagation is difficult.
          其疲劳裂纹的稳定扩展也较难形成典型的疲劳条带。
        • The fatigue stresses can be estimated with striation widths on fracture surface for Titanium alloys under experimental and service conditions.
          对钛合金在实验和工程应用条件下的构件进行断口定量反推,研究疲劳条带间距反推疲劳应力在钛合金应用的可行性。